| MOQ: | 1PCS |
| Price: | USD9.99-99.99 |
| Standard Packaging: | Vacuum bags+Cartons |
| Delivery Period: | 8-9 working days |
| Payment Method: | T/T |
| Supply Capacity: | 5000PCS per month |
This 4-layer PCB uses a stack-up of two 20mil RF-35TC cores bonded with a 5mil WL-PP280 film. The finished board measures 1.3mm thick, with 1oz copper on every layer. It comes with immersion gold surface finish and white silkscreen. Blind vias are formed between layer 3 and layer 4, and the single board size is 47.5 mm × 62.4 mm. It is built for high-power RF work that demands low signal loss and dependable heat dissipation.
Construction details
| Item | Specification |
| Layer count | 4 layers |
| Stack-up | 20mil RF-35TC + 5mil WL-PP280 + 20mil RF-35TC |
| Finished thickness | 1.3 mm |
| Copper weight | 1 oz per layer |
| Board dimension | 47.5 mm × 62.4 mm, 1PCS |
| Surface finish | Immersion gold |
| Silkscreen | White marking |
| Via type | Blind vias 3-4 |
| Quality check | 100% electrical inspection before shipment |
Stack-up
![]()
RF-35TC Laminate Introduction
RF-35TC is a thermally conductive low-loss laminate, filled with ceramic and reinforced by fiberglass within a PTFE base. It delivers top-tier loss tangent and solid thermal transfer, and its dielectric constant stays steady across wide temperature ranges. The material helps boost antenna gain and efficiency, and bonds well to very low-profile copper to cut insertion loss.
It is intended for high-power applications where even minor signal loss matters. The substrate pulls heat away from transmission lines and surface-mounted parts like transistors and capacitors. Unlike hydrocarbon alternatives, RF-35TC will not oxidize, turn yellow, or see upward drift in Dk and Df over time. Its low Z-axis CTE keeps performance stable for narrowband and broadband couplers, while restrained X/Y CTE maintains critical spacing between traces on printed filters. Its dissipation factor sits at 0.0011, paired with strong thermal conductivity, making it a natural pick for power amplifiers.
Thermal conductivity readings change based on test methods. Copper-clad samples usually return higher values because copper reduces contact resistance between the sample and test gear. Even when tested without copper cladding, RF-35TC keeps strong thermal performance, and its low Df separates it from other thermally conductive substrates.
![]()
Benefits of RF-35TC Material
Applications
DATA SHEET
| RF-35TC TYPICAL VALUES | |||||
| Property | Test Method | Unit | Value | Unit | Value |
| DK at 10 GHz | IPC-650 2.5.5.5.1(modified) | 3.5 | 3.5 | ||
| Tck(-30 to 120℃) | IPC-650 2.5.5.5.1(modified) | ppm | 24 | ppm | 24 |
| Df at 10 GHz | IPC-650 2.5.5.5.1(modified) | 0.0011 | 0.0011 | ||
| Dielectric Breakdown | IPC-650 2.5.6(in-Plane,Two Pins in Oil) | kV | 56.7 | kV | 56.7 |
| Dielectric Strength | ASTM D 149(Through Plane) | V/mil | 570 | V/mm | 22,441 |
| Arc Resistance | IPC-650 2.5.1 | Seconds | 304 | Seconds | 304 |
| Moisture Absorption | IPC-650 2.6.2.1 | % | 0.05 | % | 0.05 |
| Flexural Strength(MD) | ASTM D 790/IPC-650 2.4.4 | psi | 12,900 | N/mm2 | 88.94 |
| Flexural Strength(CD) | ASTM D 790/IPC-650 2.4.4 | psi | 11,700 | N/mm2 | 80.67 |
| Tensile Strength(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 9,020 | N/mm2 | 62.19 |
| Tensile Strength(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 7,740 | N/mm2 | 53.37 |
| Elongation at Break(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | % | 1.89 | N/mm | 1.89 |
| Elongation at Break(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | % | 1.7 | % | 1.7 |
| Young's Modulus(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 667,000 | N/mm2 | 4,599 |
| Young's Modulus(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 637,000 | N/mm2 | 4,392 |
| Poisson's Ratio(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | 0.18 | 0.18 | ||
| Poisson's Ratio(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | 0.23 | 0.18 | ||
| Compressive Modulus | ASTM D 695(23℃) | psi | 560,000 | N/mm2 | 3,861 |
| Flexural Strength(MD) | ASTM D 790/IPC-650 2.4.4 | psi | 1.46 x 106 | N/mm2 | 10,309 |
| Flexural Strength(CD) | ASTM D 790/IPC-650 2.4.4 | psi | 1.50 x 106 | N/mm2 | 10,076 |
| Peel Stength(½ oz.CVH) | IPC-650 2.4.8(Thermal Stress.) | Ibs./inch | 7 | g/cm3 | 1.25 |
| Thermal Conductivity(Unclad,125℃) | ASTM F433(Guarded Heat Flow) | W/(mK) | 0.6 | W/(mK) | 0.6 |
| Thermal Conductivity(C1/C1,125℃) | ASTM F433(Guarded Heat Flow) | W/(mK) | 0.92 | W/(mK) | 0.92 |
| Thermal Conductivity(CH/CH,125℃) | ASTM F433(Guarded Heat Flow) | W/(mK) | 0.87 | W/(mK) | 0.87 |
| Dimensional Stability(MD) | IPC-650-2.4.39 Sec.5.4(After Etch) | mils/in. | 0.23 | mm/M | 0.23 |
| Dimensional Stability(CD) | IPC-650-2.4.39 Sec.5.4(After Etch) | mils/in. | 0.64 | mm/M | 0.64 |
| Dimensional Stability(MD) | IPC-650-2.4.39 Sec.5.5(Thermal Stress.) | mils/in. | -0.04 | mm/M | -0.04 |
| Dimensional Stability(CD) | IPC-650-2.4.39 Sec.5.5(Thermal Stress.) | mils/in. | 0.46 | mm/M | 0.46 |
| Surface Resistivity | IPC-650 2.5.17.1(after elevated temp.) | Mohms | 8.33 x 107 | Mohms | 8.33 x 107 |
| Surface Resistivity | IPC-650 2.5.17.1(after humidity) | Mohms | 6.42 x 107 | Mohms | 6.42 x 107 |
| Volume Resistivity | IPC-650 2.5.17.1(after elevated temp.) | Mohms/cm | 5.19 x 108 | Mohms/cm | 5.19 x 108 |
| Volume Resistivity | IPC-650 2.5.17.1(after humidity) | Mohms/cm | 2.91 x 108 | Mohms/cm | 2.91 x 108 |
| CTE(X axis)(25-260℃) | IPC-650 2.4.41/ASTM D 3386 | ppm/℃ | 11 | ppm/℃ | 11 |
| CTE(Y axis)(25-260℃) | IPC-650 2.4.41/ASTM D 3386 | ppm/℃ | 13 | ppm/℃ | 13 |
| CTE(Z axis)(25-260℃) | IPC-650 2.4.41/ASTM D 3386 | ppm/℃ | 34 | ppm/℃ | 34 |
| Density | ASTM D 792 | g/cm3 | 2.35 | g/cm3 | 2.35 |
| Hardness | ASTM D 2240(Shore D) | 79.1 | 79.1 | ||
| Strain at Break(MD) | ASTM D 790/IPC-650 2.4.4 | % | 0.014 | % | 0.014 |
| Strain at Break(CD) | ASTM D 790/IPC-650 2.4.4 | % | 0.013 | % | 0.013 |
| Specific Heat | ASTM E 1269-05,E 967-08,E968-02 | j/(g℃) | 0.94 | j/(g℃) | 0.94 |
| Td(2% Weight Loss) | IPC-650 2.4.24.6/TGA | oF | 788 | ℃ | 420 |
| Td(5% Weight Loss) | IPC-650 2.4.24.6/TGA | oF | 817 | ℃ | 436 |
What is WL-PP280
WL-PP280 is a fiberglass-free ceramic composite bonding film. Thermoset resin coats both sides of ceramic-filled PTFE film, combining the reliable dielectric behaviour of PTFE ceramic film with the good processing characteristics of thermoset resin. It meets the tough requirements of complex microwave multilayer PCBs, including repeated lamination, via plugging, controlled resin flow, low-temperature pressing, stable bonding and easy handling.
Compared against common high-frequency prepregs such as Speed C, FEP, PFA and hydrocarbon fiberglass materials, WL-PP280 improves production yield and long-term reliability for microwave multilayer structures, with good overall cost performance.
Features
This 4-layer blind-via PCB uses RF-35TC cores together with WL-PP280 bonding film, offering a practical solution for high-power RF systems. It balances ultra-low RF loss, effective thermal spreading and stable multilayer lamination, fitting power amplifiers, satellite communication links and high-performance antenna systems. Send over your gerber files for a quote.
![]()
![]()
| MOQ: | 1PCS |
| Price: | USD9.99-99.99 |
| Standard Packaging: | Vacuum bags+Cartons |
| Delivery Period: | 8-9 working days |
| Payment Method: | T/T |
| Supply Capacity: | 5000PCS per month |
This 4-layer PCB uses a stack-up of two 20mil RF-35TC cores bonded with a 5mil WL-PP280 film. The finished board measures 1.3mm thick, with 1oz copper on every layer. It comes with immersion gold surface finish and white silkscreen. Blind vias are formed between layer 3 and layer 4, and the single board size is 47.5 mm × 62.4 mm. It is built for high-power RF work that demands low signal loss and dependable heat dissipation.
Construction details
| Item | Specification |
| Layer count | 4 layers |
| Stack-up | 20mil RF-35TC + 5mil WL-PP280 + 20mil RF-35TC |
| Finished thickness | 1.3 mm |
| Copper weight | 1 oz per layer |
| Board dimension | 47.5 mm × 62.4 mm, 1PCS |
| Surface finish | Immersion gold |
| Silkscreen | White marking |
| Via type | Blind vias 3-4 |
| Quality check | 100% electrical inspection before shipment |
Stack-up
![]()
RF-35TC Laminate Introduction
RF-35TC is a thermally conductive low-loss laminate, filled with ceramic and reinforced by fiberglass within a PTFE base. It delivers top-tier loss tangent and solid thermal transfer, and its dielectric constant stays steady across wide temperature ranges. The material helps boost antenna gain and efficiency, and bonds well to very low-profile copper to cut insertion loss.
It is intended for high-power applications where even minor signal loss matters. The substrate pulls heat away from transmission lines and surface-mounted parts like transistors and capacitors. Unlike hydrocarbon alternatives, RF-35TC will not oxidize, turn yellow, or see upward drift in Dk and Df over time. Its low Z-axis CTE keeps performance stable for narrowband and broadband couplers, while restrained X/Y CTE maintains critical spacing between traces on printed filters. Its dissipation factor sits at 0.0011, paired with strong thermal conductivity, making it a natural pick for power amplifiers.
Thermal conductivity readings change based on test methods. Copper-clad samples usually return higher values because copper reduces contact resistance between the sample and test gear. Even when tested without copper cladding, RF-35TC keeps strong thermal performance, and its low Df separates it from other thermally conductive substrates.
![]()
Benefits of RF-35TC Material
Applications
DATA SHEET
| RF-35TC TYPICAL VALUES | |||||
| Property | Test Method | Unit | Value | Unit | Value |
| DK at 10 GHz | IPC-650 2.5.5.5.1(modified) | 3.5 | 3.5 | ||
| Tck(-30 to 120℃) | IPC-650 2.5.5.5.1(modified) | ppm | 24 | ppm | 24 |
| Df at 10 GHz | IPC-650 2.5.5.5.1(modified) | 0.0011 | 0.0011 | ||
| Dielectric Breakdown | IPC-650 2.5.6(in-Plane,Two Pins in Oil) | kV | 56.7 | kV | 56.7 |
| Dielectric Strength | ASTM D 149(Through Plane) | V/mil | 570 | V/mm | 22,441 |
| Arc Resistance | IPC-650 2.5.1 | Seconds | 304 | Seconds | 304 |
| Moisture Absorption | IPC-650 2.6.2.1 | % | 0.05 | % | 0.05 |
| Flexural Strength(MD) | ASTM D 790/IPC-650 2.4.4 | psi | 12,900 | N/mm2 | 88.94 |
| Flexural Strength(CD) | ASTM D 790/IPC-650 2.4.4 | psi | 11,700 | N/mm2 | 80.67 |
| Tensile Strength(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 9,020 | N/mm2 | 62.19 |
| Tensile Strength(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 7,740 | N/mm2 | 53.37 |
| Elongation at Break(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | % | 1.89 | N/mm | 1.89 |
| Elongation at Break(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | % | 1.7 | % | 1.7 |
| Young's Modulus(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 667,000 | N/mm2 | 4,599 |
| Young's Modulus(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | psi | 637,000 | N/mm2 | 4,392 |
| Poisson's Ratio(MD) | ASTM D 3039/IPC-TM-650 2.4.19 | 0.18 | 0.18 | ||
| Poisson's Ratio(CD) | ASTM D 3039/IPC-TM-650 2.4.19 | 0.23 | 0.18 | ||
| Compressive Modulus | ASTM D 695(23℃) | psi | 560,000 | N/mm2 | 3,861 |
| Flexural Strength(MD) | ASTM D 790/IPC-650 2.4.4 | psi | 1.46 x 106 | N/mm2 | 10,309 |
| Flexural Strength(CD) | ASTM D 790/IPC-650 2.4.4 | psi | 1.50 x 106 | N/mm2 | 10,076 |
| Peel Stength(½ oz.CVH) | IPC-650 2.4.8(Thermal Stress.) | Ibs./inch | 7 | g/cm3 | 1.25 |
| Thermal Conductivity(Unclad,125℃) | ASTM F433(Guarded Heat Flow) | W/(mK) | 0.6 | W/(mK) | 0.6 |
| Thermal Conductivity(C1/C1,125℃) | ASTM F433(Guarded Heat Flow) | W/(mK) | 0.92 | W/(mK) | 0.92 |
| Thermal Conductivity(CH/CH,125℃) | ASTM F433(Guarded Heat Flow) | W/(mK) | 0.87 | W/(mK) | 0.87 |
| Dimensional Stability(MD) | IPC-650-2.4.39 Sec.5.4(After Etch) | mils/in. | 0.23 | mm/M | 0.23 |
| Dimensional Stability(CD) | IPC-650-2.4.39 Sec.5.4(After Etch) | mils/in. | 0.64 | mm/M | 0.64 |
| Dimensional Stability(MD) | IPC-650-2.4.39 Sec.5.5(Thermal Stress.) | mils/in. | -0.04 | mm/M | -0.04 |
| Dimensional Stability(CD) | IPC-650-2.4.39 Sec.5.5(Thermal Stress.) | mils/in. | 0.46 | mm/M | 0.46 |
| Surface Resistivity | IPC-650 2.5.17.1(after elevated temp.) | Mohms | 8.33 x 107 | Mohms | 8.33 x 107 |
| Surface Resistivity | IPC-650 2.5.17.1(after humidity) | Mohms | 6.42 x 107 | Mohms | 6.42 x 107 |
| Volume Resistivity | IPC-650 2.5.17.1(after elevated temp.) | Mohms/cm | 5.19 x 108 | Mohms/cm | 5.19 x 108 |
| Volume Resistivity | IPC-650 2.5.17.1(after humidity) | Mohms/cm | 2.91 x 108 | Mohms/cm | 2.91 x 108 |
| CTE(X axis)(25-260℃) | IPC-650 2.4.41/ASTM D 3386 | ppm/℃ | 11 | ppm/℃ | 11 |
| CTE(Y axis)(25-260℃) | IPC-650 2.4.41/ASTM D 3386 | ppm/℃ | 13 | ppm/℃ | 13 |
| CTE(Z axis)(25-260℃) | IPC-650 2.4.41/ASTM D 3386 | ppm/℃ | 34 | ppm/℃ | 34 |
| Density | ASTM D 792 | g/cm3 | 2.35 | g/cm3 | 2.35 |
| Hardness | ASTM D 2240(Shore D) | 79.1 | 79.1 | ||
| Strain at Break(MD) | ASTM D 790/IPC-650 2.4.4 | % | 0.014 | % | 0.014 |
| Strain at Break(CD) | ASTM D 790/IPC-650 2.4.4 | % | 0.013 | % | 0.013 |
| Specific Heat | ASTM E 1269-05,E 967-08,E968-02 | j/(g℃) | 0.94 | j/(g℃) | 0.94 |
| Td(2% Weight Loss) | IPC-650 2.4.24.6/TGA | oF | 788 | ℃ | 420 |
| Td(5% Weight Loss) | IPC-650 2.4.24.6/TGA | oF | 817 | ℃ | 436 |
What is WL-PP280
WL-PP280 is a fiberglass-free ceramic composite bonding film. Thermoset resin coats both sides of ceramic-filled PTFE film, combining the reliable dielectric behaviour of PTFE ceramic film with the good processing characteristics of thermoset resin. It meets the tough requirements of complex microwave multilayer PCBs, including repeated lamination, via plugging, controlled resin flow, low-temperature pressing, stable bonding and easy handling.
Compared against common high-frequency prepregs such as Speed C, FEP, PFA and hydrocarbon fiberglass materials, WL-PP280 improves production yield and long-term reliability for microwave multilayer structures, with good overall cost performance.
Features
This 4-layer blind-via PCB uses RF-35TC cores together with WL-PP280 bonding film, offering a practical solution for high-power RF systems. It balances ultra-low RF loss, effective thermal spreading and stable multilayer lamination, fitting power amplifiers, satellite communication links and high-performance antenna systems. Send over your gerber files for a quote.
![]()
![]()