This high frequency PCB uses MT77 high-frequency laminate, arranged as a symmetrical stack-up with two 5mil MT77 cores bonded by MT77 1078 prepreg. It is a 4-layer board with 0.5 oz finished copper on inner layers and 1 oz finished copper on outer layers, delivering an ultra-thin finished board thickness of only 0.6 mm. This board is finished with ENEPIG, green solder mask and white silkscreen. The panel dimension is 127.5 mm × 77.5 mm including tooling strip, and the core process under evaluation is resin plugging followed by planar plating on vias.
Construction details
| Item | Specification |
| Layer Count | 4 layers |
| Stackup | 5mil MT77 + MT77 1078 PP + 5mil MT77 |
| Finished Board Thickness | 0.6 mm |
| Inner Finished Copper | 0.5 oz |
| Outer Finished Copper | 1 oz |
| Surface Finish | ENEPIG |
| Solder Mask & Silkscreen | Green solder mask, white silkscreen |
| Panel Dimension | 127.5 mm × 77.5 mm (tooling border included) |
| Core Process Under Evaluation | Resin plugging and planar plating |
![]()
Material Behaviour and Process Constraints of Thin MT77 High-frequency Substrate
MT77 high-frequency material maintains stable Dk and low dissipation factor across high-frequency bands, which suits compact RF and high-speed circuits. At just 0.6mm finished thickness, the substrate has low rigidity and is sensitive to thermal shock and mechanical stress compared with standard PCB materials. Every fabrication stage including lamination, resin curing, grinding and electroplating introduces heat and pressure loads. Uneven stress distribution easily leads to board warpage, layer misregistration and dimensional distortion. These defects not only disrupt the electrical consistency of high-frequency transmission lines, but also bring difficulties to subsequent via processing. The symmetrical stackup helps offset part of the thermal stress, yet the difference in copper loading between inner and outer layers still leaves residual stress that needs close tracking through production.
![]()
Key Control Points for Resin Plugging
Resin plugging forms the foundation of the full planar plating workflow on these thin high-frequency boards. Resin grade, dispense pressure, filling speed and curing profile all need fine tuning to match the delicate substrate. Excessive dispensing pressure forces resin to bleed out of via openings and contaminate adjacent circuit traces. Insufficient pressure leads to incomplete filling and trapped voids inside the vias. Voids sealed within the resin expand during temperature cycling, which may eventually cause cracking or interfacial delamination. A stepped curing cycle is applied after filling to avoid sharp temperature spikes that bend the thin core. Once fully cured, the resin creates a solid base ready for grinding.
Coplanarity Management During Planar Plating
Grinding removes excess cured resin and brings the resin surface close to the copper plane of surrounding pads. Grinding depth needs tight control. Over-grinding exposes the resin matrix and weakens bonding with the plated copper that follows. Insufficient grinding leaves obvious raised bumps on the pad surface. Copper plating then covers the resin region to form a continuous flat copper surface together with the original pad copper. Unstable plating rate creates height variation across the pad, hurting solderability and signal integrity. For high-frequency applications, irregular copper geometry around filled vias can also introduce unwanted impedance shifts.
Reliability Validation of ENEPIG Surface Finish
ENEPIG is selected for its good tarnish resistance, reliable solderability and tolerance to repeated soldering cycles. The full sequence of resin filling, grinding and plating exposes the substrate to multiple thermal runs. This test board lets us check whether the ENEPIG finish maintains good adhesion without peeling, discoloration or micro-cracks after all these operations. The boundary where plated copper meets filled resin is the key inspection zone. Tiny gaps or micro-seams at this junction can trap flux residue and develop reliability risks over long service time.
Practical Value of This High Frequency PCB
This 4-layer ultra-thin MT77 PCB is built specifically for process development on resin plugging and planar plating. It generates real production data to define a stable process window, balancing substrate flatness, high-frequency electrical stability, coplanarity of filled vias and surface finish reliability. The process insights collected from this sample support volume manufacturing of miniaturized RF modules that require ultra-thin stack construction, flat filled vias and consistent high-frequency performance.
![]()
![]()
| MOQ: | 1PCS |
| Price: | USD9.99-99.99 |
| Standard Packaging: | Vacuum bags+Cartons |
| Delivery Period: | 8-9 working days |
| Payment Method: | T/T |
| Supply Capacity: | 5000PCS per month |
This high frequency PCB uses MT77 high-frequency laminate, arranged as a symmetrical stack-up with two 5mil MT77 cores bonded by MT77 1078 prepreg. It is a 4-layer board with 0.5 oz finished copper on inner layers and 1 oz finished copper on outer layers, delivering an ultra-thin finished board thickness of only 0.6 mm. This board is finished with ENEPIG, green solder mask and white silkscreen. The panel dimension is 127.5 mm × 77.5 mm including tooling strip, and the core process under evaluation is resin plugging followed by planar plating on vias.
Construction details
| Item | Specification |
| Layer Count | 4 layers |
| Stackup | 5mil MT77 + MT77 1078 PP + 5mil MT77 |
| Finished Board Thickness | 0.6 mm |
| Inner Finished Copper | 0.5 oz |
| Outer Finished Copper | 1 oz |
| Surface Finish | ENEPIG |
| Solder Mask & Silkscreen | Green solder mask, white silkscreen |
| Panel Dimension | 127.5 mm × 77.5 mm (tooling border included) |
| Core Process Under Evaluation | Resin plugging and planar plating |
![]()
Material Behaviour and Process Constraints of Thin MT77 High-frequency Substrate
MT77 high-frequency material maintains stable Dk and low dissipation factor across high-frequency bands, which suits compact RF and high-speed circuits. At just 0.6mm finished thickness, the substrate has low rigidity and is sensitive to thermal shock and mechanical stress compared with standard PCB materials. Every fabrication stage including lamination, resin curing, grinding and electroplating introduces heat and pressure loads. Uneven stress distribution easily leads to board warpage, layer misregistration and dimensional distortion. These defects not only disrupt the electrical consistency of high-frequency transmission lines, but also bring difficulties to subsequent via processing. The symmetrical stackup helps offset part of the thermal stress, yet the difference in copper loading between inner and outer layers still leaves residual stress that needs close tracking through production.
![]()
Key Control Points for Resin Plugging
Resin plugging forms the foundation of the full planar plating workflow on these thin high-frequency boards. Resin grade, dispense pressure, filling speed and curing profile all need fine tuning to match the delicate substrate. Excessive dispensing pressure forces resin to bleed out of via openings and contaminate adjacent circuit traces. Insufficient pressure leads to incomplete filling and trapped voids inside the vias. Voids sealed within the resin expand during temperature cycling, which may eventually cause cracking or interfacial delamination. A stepped curing cycle is applied after filling to avoid sharp temperature spikes that bend the thin core. Once fully cured, the resin creates a solid base ready for grinding.
Coplanarity Management During Planar Plating
Grinding removes excess cured resin and brings the resin surface close to the copper plane of surrounding pads. Grinding depth needs tight control. Over-grinding exposes the resin matrix and weakens bonding with the plated copper that follows. Insufficient grinding leaves obvious raised bumps on the pad surface. Copper plating then covers the resin region to form a continuous flat copper surface together with the original pad copper. Unstable plating rate creates height variation across the pad, hurting solderability and signal integrity. For high-frequency applications, irregular copper geometry around filled vias can also introduce unwanted impedance shifts.
Reliability Validation of ENEPIG Surface Finish
ENEPIG is selected for its good tarnish resistance, reliable solderability and tolerance to repeated soldering cycles. The full sequence of resin filling, grinding and plating exposes the substrate to multiple thermal runs. This test board lets us check whether the ENEPIG finish maintains good adhesion without peeling, discoloration or micro-cracks after all these operations. The boundary where plated copper meets filled resin is the key inspection zone. Tiny gaps or micro-seams at this junction can trap flux residue and develop reliability risks over long service time.
Practical Value of This High Frequency PCB
This 4-layer ultra-thin MT77 PCB is built specifically for process development on resin plugging and planar plating. It generates real production data to define a stable process window, balancing substrate flatness, high-frequency electrical stability, coplanarity of filled vias and surface finish reliability. The process insights collected from this sample support volume manufacturing of miniaturized RF modules that require ultra-thin stack construction, flat filled vias and consistent high-frequency performance.
![]()
![]()